If cold pulls won't work get a new nozzle. Filament of choice for this procedure is Nylon.

One of the alternatives could be THF to dissolve the plastic and go from there. Don't know what Prusa charges for nozzles but it can't be that bad to make this procedure worth it. After all it is a Prusa and not some industrial machine.